The international General Conference Pottery honor introduces ceramic work. The SHAB test documented by Digitalfire uses bars and marks to investigate shrinkage and other properties. Here, an instructor guides a drying observation only, without a kiln.

Mark the sample before it dries

Advertisementpreview

Use known modeling clay selected by the responsible adult. Form a small bar with reasonably uniform thickness on a surface that allows drying without holding or stretching the material. A food dough cannot establish how a different ceramic clay will behave.

While the sample is wet, make two discreet marks 100 millimeters apart if its size allows. Measure and record the actual interval rather than assuming the ruler was positioned perfectly. You will track the distance between the marks, not an irregular outer edge.

Wait and measure the same interval

Label the sample with the clay type and date. Let it dry as instructed, without trying to accelerate the process using improvised equipment. Digitalfire’s explanation of drying shrinkage describes how materials and conditions can produce different behavior.

When the adult judges the sample dry, measure between the same marks again. Keep the same unit and record separate “wet” and “dry” columns. Note any warping or cracking between the marks; that sample might not provide a reliable comparison.

Calculate with an example

Imagine an initial interval of 100 millimeters and a dry interval of 94 millimeters. The reduction is 6 millimeters. Because the initial distance was 100, the example’s linear drying shrinkage is 6%.

In general, divide the reduction by the initial distance and multiply by 100. If another interval begins at 50 millimeters and ends at 47, its 3 millimeter reduction is also 6%. A shorter sample can lose fewer millimeters while showing the same proportional change.

Read alsoScience in Quito: explore backpack strap pressure with your Pathfinder unit

Why use marks rather than the whole object?

Advertisementpreview

Edges can be rounded during shaping or lose a fragment during handling. Defined marks help preserve the points being compared. They do not remove every possible error, but they make the measurement question more precise.

Ask two people to read the ruler independently. If one finds 94 and another 97 millimeters, check the ruler’s starting point and the chosen marks. Do not average the readings before understanding the discrepancy. Measuring between different points is not simply variation in the clay.

Drying is not firing

A dry bar has not yet undergone ceramic firing. This observation alone does not establish its final size after a kiln firing. Do not promise that a lid will fit a fired pot just because the dry measurements look right.

Label the record “wet-to-dry comparison; not fired.” If the instructor conducts a later stage at suitable facilities, that needs its own measurements and recorded conditions. Separating the stages avoids combining two transformations into one unexplained number.

When presenting, show both measurements, the reduction and the proportional calculation. Add a design decision: test the same clay first rather than copy another material’s percentage. The measurement becomes useful when it informs the next modeling choice.

Keep a sketch showing exactly where the marks were made. Another group should be able to repeat the reading without asking which edges you used. If a mark disappears, record that limitation and prepare a new sample instead of reconstructing an unverifiable distance from memory.